Coatings – Safe Touch

Coatings – Safe Touch

Shown here is the t971 aerolon coating after application, this specially designed coating has aerogel in it which gives the temperature resistance for safe touch conditions, now the personnel can lean on this pipe while they turn off the control behind it and not burn...
Maintenance

Maintenance

Tnemec 215 is used here to fill cracks in the concrete to ensure that safe drinking water does not seep into the concrete and release salts back into potable water.
Maintenance

Maintenance

Specialized potable water lining system by Tnemec utilize T215 and t217 to seal the surface and recreate a new liner inside this concrete tank, Utilized by the City of St. John’s, NL
Metal Roof Paints

Metal Roof Paints

When heights are involved, don’t trust simple epoxy poly systems and risk major overspray, trust the professionals with LDG to Specify specialed metal/aluminum coatings that Minimize...
Industriel Floors

Industriel Floors

From simple epoxy systems to resin rich aggregate systems. Specialized Polyaspartic non yellowing, long lasting finishes in a resinous mix.
Fireproofing

Fireproofing

Shown, Test trials of the Famous Jotun 1709 mesh-free fire retardant system, now being specified by worldwide companies and used by many coating applicators in the Southern USA in the tune of millions of dollars, let us work with you on specifying this...
Air Liquid Amherst, NS

Air Liquid Amherst, NS

Amherst, NS, after sandblasting or grinding bare steel is spot primed with  Zinc coating to give maximum coating life like d302.
Delta / Marriott Fredericton

Delta / Marriott Fredericton

The Metal Roof was refinished with t115 Hybird primer and t1028 Industriel dryfall by Tnemec distributed by LDG Sales.
Delta / Marriott Fredericton – Metal Roof Paints

Delta / Marriott Fredericton – Metal Roof Paints

 Original surface before painting, it appears that original metal surface either failed or was attempted to be painted, sp2 Hand Sanding with sponges allowed us to feather the edges to ensure tight edges for priming, then all spots were primed before 2 coats of...
Call Now ButtonCall